Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics LNP COLORCOMP AX98567H ABS LNP* COLORCOMP* AX98567H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | |
LATI Latamid 66 H2 G/35-V0HF1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 120 °C, Time 720000 sec |
33.3 ft-lb/in² @Temperature 248 °F, Time 200 hour |
after aging water/glycol; ISO 179/1eU |
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | ISO 179 |
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0 Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15 Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 S PA6-GF30 Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-15 PA6-GF15 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65 Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40 Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSGK-30/4 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X/4 is a heat stabilized PA 66 + PA 6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30/4 X has the foll.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSM-30/2 PA666-MD30 Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30 Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30 Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl.. |
|||
Charpy Impact Unnotched | >= 7.00 J/cm² | >= 33.3 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | |
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
|
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe) Very easy-flowing, impact-modified grade.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | ISO 179/1eU |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT Description: Is a PBT, injection-molding grade with 30% glass fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance, e.g. automotive connect.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | ISO 179 |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | ISO 179 |
BASF Ultramid® 82335G HS BK 102 50% Glass Filled PA6 (Dry) Description: Ultramid 8235G HS BK-102 is a heat stabilized, pigmented black, 50% glass fiber reinforced PA6 injection molding compound offering excellent level of strength, stiffness, high temperatu.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² | 33.3 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 7.00 J/cm² @Temperature 30.0 °C |
33.3 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |