Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
Charpy Impact Unnotched | 6.70 J/cm² @Temperature 23.0 °C |
31.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² @Temperature 135 °C, Time 720000 sec |
31.9 ft-lb/in² @Temperature 275 °F, Time 200 hour |
after aging water/glycol; ISO 179/1eU |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | DAM; ISO 179/1eU |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² @Temperature -20.0 °C |
31.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Xmod™ PC75 High Crystalline Polypropylene Copolymer Xmod PC75 is a HCPP intended for injection molding of automotive interior parts. Xmod PC75 is a very easy-flowing material combined with a good balance between impact strength and stiffness. The m.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² @Temperature -30.0 °C |
31.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | 23°C, Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Charpy Impact Unnotched | 6.70 J/cm² | 31.9 ft-lb/in² | ISO 179/1eU |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |