Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK603 BK851 PBT
(Unverified Data**) Crastin® SK603 BK851 is a 20% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179 |
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66 Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 HH-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -40.0 °C |
26.2 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 HS-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1U |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7278 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4130 XF 700051 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowability |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | |
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | |
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | |
LATI Latilub 66-20T PA66, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | |
LATI Latiohm 73/23-10 CNT POM Semiconductive/dissipative product based on Polyoxymethylene (POM). Carbon nanotubes.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -20.0 °C |
26.2 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Nepol™ GB402HP 40% Long Glass Fiber Reinforced Polypropylene Nepol GB402HP is a 40% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -20.0 °C |
26.2 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 30.0 °C |
26.2 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 FC PA6-GF30 Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface .. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66... |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1146 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 7423-2 NF3001 13% Glass Filled PA66 (Dry) Ultramid 7423-2 NF3001 is an impact modified, 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179 |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eU |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® TV4 491 (PBT+PET)-GF50 |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179-1 |
Unitika EX-1020K PA6, Dry Conducting nylonInformation provided by Unitika Ltd. |