| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Unitika EX-1020K PA6, Dry.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
| Water Absorption | 1.3 % @Time 86400 sec |
1.3 % @Time 24.0 hour |
ISO 62 |
| Moisture Absorption at Equilibrium | 2.0 % | 2.0 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.010 cm/cm @Thickness 3.20 mm |
0.010 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm @Thickness 3.20 mm |
0.012 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 110 | 110 | ISO 2039 |
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ISO 527-1/-2 |
| Elongation at Break | 80 % | 80 % | ISO 527-1/-2 |
| Elongation at Yield | 4.0 % | 4.0 % | ISO 527-1/-2 |
| Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
| Flexural Strength | 80.0 MPa | 11600 psi | ISO 178 |
| Flexural Modulus | 2.50 GPa | 363 ksi | ISO 178 |
| Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179-1 |
| Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 147 °C | 297 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 10 ohm-cm | 10 ohm-cm | IEC 60093 |