Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PC 11 N PP, imp. strength Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A USZ200 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A USZ200 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**) Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 HI HV TS PA6 with impact modifier PA 6 higher viscosity, heat stabilized, impact modified for extrusion and blow molding. Automotive applications as air ducts and fuel filter pipes, fuel and oil containers.Information Provided by Pl.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 LI PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature -20.0 °C |
40.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 LI PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-TP4 (Cond.) Impact Modified Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-TP4 Impact Modified Nylon 66 (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-TP4 Impact Modified Nylon 66 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eA |
Lanxess Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66 PA 66, non-reinforced, injection molding, improved flowability, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax ATE70-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned) Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Styrolution Terblend® N NM-21 XP ABS+PA (Conditioned) Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NB40 NL IH PA 6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® EH 501 Polypropylene Impact Copolymer Made for extrusion applications. LHTA stabilization. Impact copolymer.Information provided by Unipetrol RPA |