| Category | Polymer , Thermoplastic , Polypropylene (PP) | 
| Manufacturer | Unipetrol RPA | 
| Trade Name | PP MONSTEN® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Unipetrol PP MONSTEN® EH 501 Polypropylene Impact Copolymer.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Melt Flow |           0.50           g/10 min           @Load 2.16 kg, Temperature 230 °C  | 
                  0.50           g/10 min           @Load 4.76 lb, Temperature 446 °F  | 
        ISO 1133 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 26.0 MPa | 3770 psi | ISO 527 | 
| Elongation at Break | >= 200 % | >= 200 % | ISO 527 | 
| Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 | 
| Charpy Impact, Notched |           1.00           J/cm²           @Temperature -20.0 °C  | 
                  4.76           ft-lb/in²           @Temperature -4.00 °F  | 
        ISO 179 | 
|           8.50           J/cm²           @Temperature 23.0 °C  | 
                  40.5           ft-lb/in²           @Temperature 73.4 °F  | 
        ISO 179 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 54.0 °C | 129 °F | ISO 75 | 
| Vicat Softening Point | 150 °C | 302 °F | ISO 306 |