Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 GF 15 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 15% glass fiber. Application: applied in automotive, electrical, engineering and consumer-goods industry, eg.: grips for electro tools, hobby tools, gears.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 32 A PA66 PA66 basic type for injection molding, compounding, extrusion. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivere.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 71 T 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrin.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant FeaturesModified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfil.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRM 1 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GF 15 GB 25 TS PA66, 15% glass fibre, 25% glass beads FeaturesPA 66 chemically reinforced with 15 % glass fibre and with the content of 25% glass beads, thermo stable. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical p.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Qualchem Danamid FEH Polyamide 6 Heat stabilized type polyamide, for long-lasting use at 120-130°CInformation provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 15 FRA 5 Polyamide 6, 15% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP HIP8040 VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-9120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-9120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9120 is developed for producing.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability.Availability: Afri.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis RA130E-2491 Polypropylene Random Copolymer RA130E-2491 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is blue colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis RA130E-6015 Polypropylene Random Copolymer RA130E-6015 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis RA130E-6017 Polypropylene Random Copolymer RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis RA130E-6020 Polypropylene Random Copolymer RA130E-6020 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eA |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T5040 FC Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |