Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.374 - 5.34 J/cm | 0.700 - 10.0 ft-lb/in | Average value: 0.765 J/cm Grade Count:48 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Izod Impact, Notched | 2.40 - 5.34 J/cm | 4.50 - 10.0 ft-lb/in | Average value: 3.81 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.900 - 5.34 J/cm @Temperature -40.0 - 0.000 °C |
1.69 - 10.0 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 4.02 J/cm Grade Count:18 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.900 - 5.34 J/cm @Thickness 3.17 - 3.20 mm |
1.69 - 10.0 ft-lb/in @Thickness 0.125 - 0.126 in |
Average value: 4.02 J/cm Grade Count:18 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | ASTM D256 |
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Izod Impact, Notched | 4.27 - 5.34 J/cm | 8.00 - 10.0 ft-lb/in | ASTM D256 |
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Izod Impact, Notched | 4.27 - 5.34 J/cm | 8.00 - 10.0 ft-lb/in | ASTM D256 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | ASTM D256 |
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl.. |
|||
Izod Impact, Notched | 4.27 - 5.34 J/cm | 8.00 - 10.0 ft-lb/in | ASTM D256 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Izod Impact, Notched | 4.81 - 5.34 J/cm | 9.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Izod Impact, Notched | 2.14 - 5.34 J/cm | 4.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
Izod Impact, Notched | 3.74 - 5.34 J/cm | 7.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Izod Impact, Notched | 4.27 - 5.34 J/cm | 8.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC T12-15541 General Purpose Molding Compound BMC T12 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Izod Impact, Notched | 0.910 - 5.34 J/cm | 1.70 - 10.0 ft-lb/in | Average value: 3.04 J/cm Grade Count:89 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched | 4.27 - 5.34 J/cm | 8.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |