| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
|
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Temperature -50.0 °C
|
9.00
ft-lb/in <br>@Temperature -58.0 °F
|
0.125 in; ASTM D256 |
|
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Temperature -50.0 °C
|
9.00
ft-lb/in <br>@Temperature -58.0 °F
|
0.125 in; ASTM D256 |
|
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
|
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | Crosswise; ASTM D256 |
|
G-11 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e..
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Temperature -28.9 °C
|
9.00
ft-lb/in <br>@Temperature -20.0 °F
|
ASTM D256 |
|
M. Holland Company PCAB250 Acrylonitrile Butadiene Styrene + PC
High heat resistanceHigh impact resistanceLow temperature impact resistanceApplications: Automotive
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
|
Ineos TUB 121N HDPE
TUB121N is a natural high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. When blended with an approved black concentrate, t..
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | Edgewise (CW); ASTM D256 |
|
Haysite H515 Polyester, High Temp Flex
H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t..
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | Edgewise (CW); ASTM D256 |
|
Haysite HTF Polyester, High Temp Flex
HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te..
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | 73°F; ASTM D256 |
|
Spartech Royalite R922 PC/ABS Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Thickness 3.17 mm
|
9.00
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin..
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Thickness 3.17 mm
|
9.00
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Techmer ES Plastiblend® PC/ABS 8800
Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc.
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Thickness 3.17 mm
|
9.00
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
|
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Thickness 3.17 mm
|
9.00
ft-lb/in <br>@Thickness 0.125 in
|
ASTM D256 |
|
PlastxWorld CEVIAN® S3100 PC/ABS alloy
Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
|
CPC - Vycom Corzan® CPVC Chlorinated PVC
Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup..
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Thickness 3.17 mm,<br> Temperature 23.0 °C
|
9.00
ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F
|
bar; ASTM D256 |
|
Diamond Polymers ABS 9301
Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc.
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Thickness 3.17 mm,<br> Temperature 23.0 °C
|
9.00
ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F
|
bar; ASTM D256 |
|
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
|
Asia Technology Pioneers CAP 501 PP Nanocomposite
Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim..
|
|||
| Izod Impact, Notched | 4.81 - 5.87 J/cm | 9.00 - 11.0 ft-lb/in | |
|
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol..
|
|||
| Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
|
Chase Plastics CP Pryme® PCA100 Polycarbonate/ABS Alloy
Information provided by Chase Plastics.
|
|||
| Izod Impact, Notched |
4.81
J/cm <br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
|
9.00
ft-lb/in <br>@Thickness 0.250 in,<br> Temperature 73.4 °F
|
Method A, Injection Molded; ASTM D256 |
|
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Izod Impact, Notched | 4.81 - 7.47 J/cm | 9.00 - 14.0 ft-lb/in | ASTM D256 |
|
Premix Premi-Glas® 1200H-24 Polyester SMC
(discontinued **)
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni..
|
|||
| Izod Impact, Notched | 4.81 - 5.87 J/cm | 9.00 - 11.0 ft-lb/in | |
|
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound
BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi..
|
|||