Polymer Property : Izod Impact, Notched = 4.81 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.81 J/cm
9.01 ft-lb/in
ASTM D256-93a
Multibase Multi-Pro® 5014 CU W Calcium Carbonate Filled Polypropylene
Multi-Pro 5014 CU W is a calcium carbonate reinforced PP concentrate with balanced impact and stiffness properties. This product is specially formulated for lawn furniture, suitable for outdoor exp..
Izod Impact, Notched 4.81 J/cm
9.01 ft-lb/in
ASTM D-256
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
73°F, 0.125 in; ASTM D256
Ravago Manufacturing Americas Hylac® GP48 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
Crosswise; ASTM D256
G-11 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e..
Izod Impact, Notched 4.81 J/cm

@Temperature -28.9 °C
9.00 ft-lb/in

@Temperature -20.0 °F
ASTM D256
M. Holland Company PCAB250 Acrylonitrile Butadiene Styrene + PC
High heat resistanceHigh impact resistanceLow temperature impact resistanceApplications: Automotive
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
Ineos TUB 121 HDPE
TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
Ineos TUB 121N HDPE
TUB121N is a natural high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. When blended with an approved black concentrate, t..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
Edgewise (CW); ASTM D256
Haysite H515 Polyester, High Temp Flex
H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
Edgewise (CW); ASTM D256
Haysite HTF Polyester, High Temp Flex
HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
73°F; ASTM D256
Spartech Royalite R57 FR/ABS Aircraft Grade Sheet
Description: Aircraft Grade SheetInformation provided by Spartech.
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm
9.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm
9.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
PlastxWorld CEVIAN® S3100 PC/ABS alloy
Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
CPC - Vycom Corzan® CPVC Chlorinated PVC
Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup..
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
9.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS 9301
Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
9.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ABS/PC 7901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
9.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
bar; ASTM D256
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Izod Impact, Notched 4.81 J/cm

@Thickness 3.17 mm
9.01 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers ASAPC TA-45
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 4.81 J/cm
9.01 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® P114WO PBT Polyester
A high impact polyester with low shrinkage, flame retardant.Data provided by the manufacturer
Izod Impact, Notched 4.81 - 5.34 J/cm
9.00 - 10.0 ft-lb/in
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
Asia Technology Pioneers CAP 501 PP Nanocomposite
Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim..
Izod Impact, Notched 4.81 J/cm
9.00 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® PCA100 Polycarbonate/ABS Alloy
Information provided by Chase Plastics.
Izod Impact, Notched 4.81 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
9.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Izod Impact, Notched 4.81 - 5.87 J/cm
9.00 - 11.0 ft-lb/in
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound
BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi..