Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® MG38U ABS High impact ABS. UL 746C f1 listed. Toughness/rigidity. Good fatigue resistance. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF40-PA12 Nylon 12, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Izod Impact, Notched | 3.74 - 6.9407 J/cm @Temperature -50.0 - 0.000 °C |
7.01 - 13.003 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 4.02 J/cm Grade Count:10 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256-93a |
Multibase Multi-ABS 801 Natural Extrusion Grade Data provided by Multibase. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM Data |
Styron Pulse® 600 ABS + Polycarbonate PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat res.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature -50.0 °C |
7.01 ft-lb/in @Temperature -58.0 °F |
ASTM Data |
Styron CALIBRE™ IM 401 18 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM 401 polycarbonate resins exhibit an excellent balance of impact strength an.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature -50.0 °C |
7.01 ft-lb/in @Temperature -58.0 °F |
ASTM Data |
Dow Prevail® 3150 ABS + Polyurethane PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527LD-45LG Nylon 66, 45% Long Glass Fiber Reinforced Long glass fiber reinforced impact modified Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced r.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B901 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B908 , 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm |
7.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color.. |
|||
Izod Impact, Notched | 3.74 J/cm @Temperature 23.0 °C |
7.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 3.74 - 13.9 J/cm @Temperature -50.0 - -50.0 °C |
7.01 - 26.0 ft-lb/in @Temperature -58.0 - -58.0 °F |
Average value: 8.37 J/cm Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |