Mechanical Properties Metric English Comments
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D-256
PlastiComp Velocity® LCF40-PA6 High Flow Nylon 6, 40% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256-56
Rotuba 855, Slow Burning Ethyl Cellulose
Data provided by the manufacturer.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
1/8 in specimen; ASTM D256
Network Polymers Nylon 6015 G33HSL
High Impact Nylon (33% Glass Fiber)Information provided by Network Polymers Inc.
Izod Impact, Notched 2.24 J/cm

@Temperature 23.0 °C
4.20 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant
Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
73°F, 0.125 in; ASTM D256
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Izod Impact, Notched 2.24 - 7.4746 J/cm

@Temperature -40.0 - -28.9 °C
4.20 - 14.003 ft-lb/in

@Temperature -40.0 - -20.0 °F
Average value: 4.31 J/cm Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Izod Impact, Notched 2.24 J/cm

@Diameter 3.17 mm
4.20 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Ineos Nova FX510 Super High Impact Polystyrene  (discontinued **)
Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi..
Izod Impact, Notched 2.24 J/cm

@Diameter 3.17 mm
4.20 ft-lb/in

@Diameter 0.125 in
bar, 0.010" notch radius; ASTM D256
Ineos Nova 6200 Super High Impact Polystyrene
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
Izod Impact, Notched 2.24 J/cm

@Diameter 3.17 mm
4.20 ft-lb/in

@Diameter 0.125 in
bar, 0.010" notch radius; ASTM D256
Ineos Nova 6201 Super High Impact Polystyrene
Good toughness, Deep draw, Easy processing using all conventional methodsApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined..
Izod Impact, Notched 2.24 J/cm

@Temperature -40.0 °C
4.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
SABIC Innovative Plastics NORYL STN15HF PPE+PS
Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing.
Izod Impact, Notched 2.24 J/cm

@Temperature -40.0 °C
4.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
SABIC Innovative Plastics NORYL STN15HF PPE+PS (Asia Pacific)
Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX1391 PPE+PS
PPE+PS blend. Unfilled. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX1391 PPE+PS (Asia Pacific)
Automotive applications, primarily. Excellent electrical properties. high heat. 305F (152C) DTUL.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific)
LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Notched 2.24 J/cm

@Thickness 3.17 mm
4.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
PlastxWorld CEVIAN®-V 500 ABS
Medium Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
Chase Plastics CP Pryme® A100HH ABS Molding Resin, High Heat
Information provided by Chase Plastics.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr..
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
Aclo Accucomp ABS ABS856BL High Flow Medium Impact Grade
Izod Impact, Notched 2.24 J/cm

@Temperature -40.0 °C
4.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Chem Polymer Durlex 709 IH PBT, Impact Modified
A highly impact modified PBT exhibiting excellent toughness and processability.Data provided by the manufacturer, Chem Polymer.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
Aclo Accucomp ABS ABS803L Medium Impact Grade
Izod Impact, Notched 2.24 - 16.0 J/cm
4.20 - 30.0 ft-lb/in
Average value: 9.69 J/cm Grade Count:26
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched 2.24 J/cm

@Temperature -40.0 °C
4.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
SABIC Innovative Plastics NORYL EM6100 PPE+PS (Asia Pacific)
Medium heat, high impact PPO/HIPS alloy used in the automotive industry.
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256A
Braskem TI6350WV High Impact Copolymer Polypropylene
Description: Superior low temperature impact, nucleated, antistatic.Applications: Suggested uses include furniture, toys, compounding.Process: Injection Molding.This resin meets the requirements for..
Izod Impact, Notched 2.24 J/cm
4.20 ft-lb/in
ASTM D256
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 35% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro..
Izod Impact, Notched 2.24 J/cm

@Thickness 3.17 mm
4.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
PlastxWorld CEVIAN® SER20 ABS
General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat..