Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.85 J/cm | 14.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature -30.0 °C |
14.7 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature -30.0 °C |
14.7 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS7R PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature -30.0 °C |
14.7 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS7R PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature -30.0 °C |
14.7 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Notched | 7.82 J/cm | 14.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DI001L PC LNP* LUBRICOMP* DI001L is a compound based on Polycarbonate resin containing 2% Silicone. Added characteristics of this grade are: Low Extractable. |
|||
Izod Impact, Notched | 7.85 J/cm | 14.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Asia Pacific) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched | 7.85 J/cm | 14.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature -30.0 °C |
14.7 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature -30.0 °C |
14.7 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.7 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Izod Impact, Notched | >= 7.85 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 14.7 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p.. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature 23.0 °C |
14.7 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-1000 General Purpose Modified PC, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | >= 7.85 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 14.7 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000HU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: Electric & Electronic (Housing, Components) For Suit caseCAS: 103598-77-2Information provided by LG Chemic.. |
|||
Izod Impact, Notched | 7.85 J/cm @Temperature 23.0 °C |
14.7 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HI-1002 High Impact Modified PC, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | >= 7.85 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 14.7 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1006FM PC, Flame Retardant Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 6.35 mm |
14.7 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® SC-1100R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GW-1010 PC, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 6.35 mm |
14.7 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® SC-1100R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3022PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022PJ is a general use grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3022R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022R is a general use grade with heat stabilizers and separating materials added.Appli.. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3025PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025PJ is a general use grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3025R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025R is a general use grade with heat stabilizers and separating materials added.Appli.. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3026PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3026PJ is an extrusion grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 7.85 J/cm | 14.7 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® H14ST Super Toughness PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Izod Impact, Notched | 7.85 J/cm | 14.7 ft-lb/in | ASTM D256 |
Cheng Yu Plastic E500G10 PC/PET, 10% Glass Fiber |
|||
Izod Impact, Notched | 7.85 J/cm | 14.7 ft-lb/in | Method A; ASTM D-256 |
Axiall 7055 Rigid PVC, Extrusion, White Georgia Gulf 7055 White is a special purpose rigid PVC extrusion compound designed for window and door applications. The compound exhibits the following characteristics: WeatherabilityChemical Res.. |
|||
Izod Impact, Notched | 7.85 J/cm @Thickness 3.17 mm |
14.7 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 450N Polymer Alloy, Blow Molding Excellent impact, formability and weather resistance.450N is a blow molding grade.Applications: ConnectorsInformation provided by Samyang. |
|||
Izod Impact, Notched | 7.85 J/cm | 14.7 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® N3040HR Nanoclay 3% Dimensional stability, Super Toughness Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |