Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 7055 Rigid PVC, Extrusion, White

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 7055 Rigid PVC, Extrusion, White.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf 7055 White is a special purpose rigid PVC extrusion compound designed for window and door applications. The compound exhibits the following characteristics: WeatherabilityChemical ResistantDurabilityEase of ProcessingToughnessInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 49.62 MPa
7197 psi
ASTM D-638
Tensile Modulus 2.73 GPa
396 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.73 GPa
396 ksi
ASTM D-790
Izod Impact, Notched 7.85 J/cm
14.7 ft-lb/in
Method A; ASTM D-256
Tensile Impact Strength 168 kJ/m²
80.0 ft-lb/in²
ASTM D-1822
Dart Drop Total Energy >= 103 J/cm
>= 0.192 ft-lb/mil
Procedure A; ASTM D-4226
>= 103 J/cm
>= 0.192 ft-lb/mil
Procedure B; ASTM D-4226
Thermal Properties Metric English Comments
CTE, linear 4.86 µm/m-°C

@Temperature -30.0 - 30.0 °C
2.70 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D-696
88.2 µm/m-°C

@Temperature 20.0 °C
49.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 66.78 °C
152.2 °F
ASTM D-648
Descriptive Properties Value Comments
Cell Classification 1-43353-22
ASTM D-4216
Users viewing this material also viewed the following: