Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.972 J/cm | 1.82 ft-lb/in | ASTM D256A |
Resinoid 2011 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
Kostat 5000 TAB Spacer Tapes PET 5000 TAB Spacer Tapes, uniquely formulated and manufactured by KOSTAT, are made of various thermoplastic substrates with ICP (Inherently Conductive Polymer) coating technology. This class of materi.. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240U PP SABIC® PPcompound G3240U is a general purpose, 40% glass filled, chemically coupled, heat stabilized and UV stabilized homopolymer polypropylene compound. The IMDS ID is 209768078. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
Izod Impact, Notched | 0.970 J/cm @Temperature -30.0 °C |
1.82 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERH PC LNP THERMOCOMP* DF002ERH is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Healthcare, Mold Release. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ERJ PC LNP THERMOCOMP* DF002ERJ is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Healthcare. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX06408 PC LNP THERMOCOMP* DX06408 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber. |
|||
Izod Impact, Notched | 0.970 J/cm @Temperature 23.0 °C |
1.82 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC LNP THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding. Mold Release |
|||
Izod Impact, Notched | 0.970 J/cm | 1.82 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific) Glass filled Nylon 12 |
|||
Izod Impact, Notched | 0.972 J/cm @Thickness 3.17 mm |
1.82 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-0802 30G Chemically Couple Glass Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | >= 0.971 J/cm @Thickness 6.35 mm |
>= 1.82 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |