Material Notes:
5000 TAB Spacer Tapes, uniquely formulated and manufactured by KOSTAT, are made of various thermoplastic substrates with ICP (Inherently Conductive Polymer) coating technology. This class of materials has distinctive advantages in ESD and cleanliness performances in comparison to other materials based on hygroscopic antistats and conductive fillers. Also, this product exhibits superior transparency and clarity that will provide a convenience of being able to inspect the components with the naked vision.Special Features:Superior Permanent Static DissipationHumidity InsensitivityLow Particle GenerationSuperior Transparency and ClarityExcellent Chemical Resistance with Environmentally Friendly MaterialsApplications:Flexible PCB FilmsDriver IC Films for TCP, COF and COG
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Flexural Strength 70.0 MPa
10200 psi
ASTM D790
Flexural Modulus 1.95 GPa
283 ksi
ASTM D790
Izod Impact, Notched 0.970 J/cm
1.82 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 158 °C
316 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible >= 85 %
>= 85 %
ASTM D1003
Electrical Properties Metric English Comments
Surface Resistivity per Square 1e+05 - 1.00e+6 ohm
1e+05 - 1.00e+6 ohm
ASTM D257