Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific) LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML6451 PC UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.69 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 5240 PR HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® HR426 PBT (Asia Pacific) AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RF0069RS PA 66 LNP THERMOCOMP* RF0069RS is a compound based on Nylon 66 resin containing Glass Fiber, Mold Release, Flame Retardant. Added features of this material include: Easy Release.This data was supplied by.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 0.000 °C |
1.69 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX92284 PP LNP* THERMOCOMP* MX92284 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers VESPEL TP-8054 Polyimide DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP KUR 4000 CH/TD Polypropylene Copolymer Polypropylene copolymer, elastomer modifiedInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 0.900 J/cm @Diameter 3.17 mm |
1.69 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5620 High Impact Polystyrene
(discontinued **) High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)