Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ AT-10CF/000 Acetal (POM) Copolymer Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Faradex DX07304 PC (Asia Pacific) CF filled grade with EMI shieldingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -40.0 °C |
0.693 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Izod Impact, Notched | 0.370 - 1.60 J/cm @Temperature -40.0 - 0.000 °C |
0.693 - 3.00 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.826 J/cm Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Flint Hills 11R12A Specialty Homopolymer Polypropylene Features: Good drop impact, radiation resistant. Product does not contain animal derived components and is phthalate-free.Applications: Injection MoldingInformation provided by Flint Hills Resour.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp OP005XXC PPS LNP LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL229 PA 66 LNP* LUBRICOMP* RAL229 is a compound based on Nylon 66 containing 10% Aramid, 10% PTFE. Added features of this grade include: Flame Retardant, Wear Resistant. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon ZE004 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006SXP PA 66 LNP* THERMOCOMP* RZ006SXP is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -30.0 °C |
0.693 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM AUT210 PEI Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 (Asia Pacific) LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -30.0 °C |
0.693 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers VESPEL TP-8161 Polyimide DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environm.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 242 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.370 - 0.690 J/cm @Temperature -40.0 - -40.0 °C |
0.693 - 1.29 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.561 J/cm Grade Count:15 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 6.35 mm |
0.693 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® CTXC-084 Polyethersulfone - Mineral Reinforced
(discontinued **) Data provided by PolyOne. |