Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Water Absorption 0.38 %
0.38 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 72.0 MPa
10400 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 3.60 GPa
522 ksi
ASTM D638
Izod Impact, Notched 0.370 J/cm

@Thickness 6.35 mm
0.693 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
ASTM D648
Flammability, UL94 V-0
V-0
CTi TESTING V-0
Processing Properties Metric English Comments
Melt Temperature 343 - 371 °C
649 - 700 °F
Stock
Mold Temperature 93.0 - 149 °C
199 - 300 °F
Drying Temperature 135 °C
275 °F