Polymer Property : Izod Impact, Notched = 0.637 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.340 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.637 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy)
VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne
Izod Impact, Notched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Faradex ES003DE PEI
LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP FARADEX ES003E PEI
LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding.
Izod Impact, Notched 0.340 - 0.534 J/cm
0.637 - 1.00 ft-lb/in
Average value: 0.469 J/cm Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP COLORCOMP EX10304C PEI (Asia Pacific)
LNP* Colorcomp* EX10304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS Technol..
Izod Impact, Notched 0.340 - 1.90 J/cm
0.637 - 3.56 ft-lb/in
Average value: 0.600 J/cm Grade Count:14
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256A
LyondellBasell Pro-fax 6331W Polypropylene Homopolymer, Antistat
Key Features: antistatic polypropylene homopolymer resin, FDA acceptable, resists dust pickup, low odor transferApplications: containers, closures, hospital and institutional ware, toysMeets FDA req..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET)
Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon.
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON MX01739C PP
LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy
E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy
E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Izod Impact, Notched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS
LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region...
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East)
Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX1736 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
Plenco 1530 Polyester, Briquette, Injection Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
Plenco 6500 Phenolic, Briquette, Injection Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM-D256
Braskem IA58 HDPE Injection Molding Polyethylene Copolymer
IA58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good ..
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
Dry; ASTM D256
Asahi Kasei Leona® CR301 Nylon 66
Suitable for a switch insulator. Low abrasion and superior electrical properties.Applications:Sliding switch insulators Information provided by Asahi Kasei
Izod Impact, Notched 0.340 J/cm
0.637 ft-lb/in
ASTM D256
Plenco 7552 Phenolic, Nodular, Injection Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..
Izod Impact, Notched 0.340 - 1.10 J/cm
0.637 - 2.06 ft-lb/in
Average value: 0.728 J/cm Grade Count:5
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 0.340 - 1.33 J/cm
0.637 - 2.50 ft-lb/in
Average value: 0.705 J/cm Grade Count:22
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..