| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.340 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.637 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
| PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy) VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne |
|||
| Izod Impact, Notched | 0.340 J/cm @Temperature 23.0 °C |
0.637 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP FARADEX ES003E PEI LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding. |
|||
| Izod Impact, Notched | 0.340 - 0.534 J/cm | 0.637 - 1.00 ft-lb/in | Average value: 0.469 J/cm Grade Count:3 |
| Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP COLORCOMP EX10304C PEI (Asia Pacific) LNP* Colorcomp* EX10304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS Technol.. |
|||
| Izod Impact, Notched | 0.340 - 1.90 J/cm | 0.637 - 3.56 ft-lb/in | Average value: 0.600 J/cm Grade Count:14 |
| Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256A |
| LyondellBasell Pro-fax 6331W Polypropylene Homopolymer, Antistat Key Features: antistatic polypropylene homopolymer resin, FDA acceptable, resists dust pickup, low odor transferApplications: containers, closures, hospital and institutional ware, toysMeets FDA req.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET) Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
| Izod Impact, Notched | 0.340 J/cm @Temperature 23.0 °C |
0.637 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| SABIC Innovative Plastics LNP Stat-kon AD000Z ABS LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region... |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Asia Pacific) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics NORYL PX1736 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| Plenco 1530 Polyester, Briquette, Injection Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM-D256 |
| Braskem IA58 HDPE Injection Molding Polyethylene Copolymer IA58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good .. |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | Dry; ASTM D256 |
| Asahi Kasei Leona® CR301 Nylon 66 Suitable for a switch insulator. Low abrasion and superior electrical properties.Applications:Sliding switch insulators Information provided by Asahi Kasei |
|||
| Izod Impact, Notched | 0.340 J/cm | 0.637 ft-lb/in | ASTM D256 |
| Plenco 7552 Phenolic, Nodular, Injection Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
| Izod Impact, Notched | 0.340 - 1.10 J/cm | 0.637 - 2.06 ft-lb/in | Average value: 0.728 J/cm Grade Count:5 |
| Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
| Izod Impact, Notched | 0.340 - 1.33 J/cm | 0.637 - 2.50 ft-lb/in | Average value: 0.705 J/cm Grade Count:22 |
| Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||