Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256A |
Total Finaclear® 521 Clear Impact Polystyrene
(discontinued **) Finaclear® 521 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with othe.. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol H200MK Polypropylene REPOL Polypropylene H200MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX11422 PA 6 LNP* KONDUIT* is a compound based on Nylon 6 resin containing thermally conductive fillers. Added feature of this material is Electrically Conductive. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 A |
Metabolix Mirel™ F1005 Injection Molding Grade PHA Bioplastic Mirel F1005 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl TN240 PPE+PS PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Asia Pacific) LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific) LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific) LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM DU319 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Asia Pacific) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS LNP* THERMOCOMP* AX08306 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS (Asia Pacific) LNP* Thermocomp* AX08306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Mineral. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WX05456 Polyester, TP LNP THERMOCOMP* WX05456 is a compound based on Polyester, TP resin containing Mineral. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature -30.0 °C |
0.487 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P.. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3443U UV Resistant Homopolymer Polypropylene DescriptionPolyfort® FPP 3443U is a 40% talc fortified UV resistant homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.260 J/cm | 0.487 ft-lb/in | ASTM D256 |
A. Schulman PP 3369-01 Polypropylene Medium-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3369-01 is a medium-flow homopolymer polypropylene nucleated and anti-static designed for the molding of thin walled, and large parts.ApplicationTypical applications of P.. |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature 23.0 °C |
0.487 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 201 Fiber Extrusion Polypropylene Applications: Staple fibers for carpets and blankets; continuous filament for ropes, cords and rugs. Information provided by Braskem |
|||
Izod Impact, Notched | 0.260 J/cm @Temperature -40.0 °C |
0.487 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 935-40M Nylon 11 A rotational molding grade Nylon 11 with a 40-50 mesh.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.260 J/cm - NB | 0.487 ft-lb/in - NB | Average value: 1.41 J/cm Grade Count:631 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |