Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers PC-1011 L Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD103R PC FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD103R PC (Europe-Africa-Middle East) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | (0.125 in); ASTM D256 |
M. Holland Company PC406R Polycarbonate Good impact resistanceGood mold releaseHigh viscosityApplications: AppliancesProtective coveringsDecorative displaysHousings |
|||
Izod Impact, Notched | 9.08 J/cm @Temperature 22.8 °C |
17.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® PC60 Polycarbonate 6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 201-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4310-6 Polycarbonate EMERGEâ„¢ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Equ.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4510-6 Polycarbonate EMERGEâ„¢ PC 4510-6 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Informa.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and .. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4510-10 Polycarbonate EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SBB 3715 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Ultra High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation P.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Westlake Plastics Zelux® M Machine Grade Polycarbonate Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Westlake Plastics Zelux® W Window Grade Polycarbonate Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ensinger Tecamid® ST Nylon (PA) Super Tough nylon, increased impact resistance and toughness over nylon 6/6.Information provided by Ensinger, Inc. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 1021 Polycarbonate A general purpose injection molding grade, natural resin. Also available as: 1021R (with release), 1023 (with UV stabilizers); 1023R (with release and UV stabilizers).Data provided by the manufactu.. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 1621 Polycarbonate A general purpose injection molding grade, natural resin, UL approved. Also available as: 1621R (with release); 1623 (with UV stabilizers); 1623R (with release and UV stabilizers).Data provided by .. |
|||
Izod Impact, Notched | 9.08 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 734-SP5 Nylon 6, Flexible Grade A highly flexible grade of Nylon 6 with outstanding impact.Data provided by the manufacturer |
|||
Izod Impact, Notched | 9.08 J/cm @Thickness 3.17 mm |
17.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPX-HTN-01043 A Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: High Temperature Strength, Impact Modified and LubricatedUL File Number: E157318Information provided by TP C.. |