Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-2010 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -20.0 °C |
10.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PTS PCA-30G00 Impact Modified Polycarbonate/PBT Alloy For Cold Temperature Impact.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -30.0 °C |
10.0 ft-lb/in @Temperature -22.0 °F |
0.125in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate Information provided by Ravago |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -30.0 °C |
10.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature 22.8 °C |
10.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | at 73°F; ASTM D256 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Ineos K38-20-188 HDPE K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural .. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | Edgewise (LW); ASTM D256 |
Haysite H515 Polyester, High Temp Flex H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high t.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.20 mm |
10.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM AR9300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | >= 5.34 J/cm @Temperature 22.8 °C |
>= 10.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP7230 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R59 ABS/PVC Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM Data |
Styron Pulse® 1310 ABS + Polycarbonate PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -50.0 °C |
10.0 ft-lb/in @Temperature -58.0 °F |
ASTM Data |
Styron CALIBRE™ IM 401 11 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 6.35 mm |
10.0 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PlastxWorld CEVIAN® DR210 PC Alloy High impact, good flowability and heat resistant.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® APC100 ABS Polycarbonate Alloy Form: PelletsInformation provided by Chase Plastics. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
Ensinger Hydex™ 202 Rigid Polyurethane (PU) Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanic.. |
|||
Izod Impact, Notched | 5.34 J/cm | 10.0 ft-lb/in | ASTM D256 |
ExxonMobil LLDPE LL 5001.09 Linear Low Density Polyethylene Resin Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending .. |
|||
Izod Impact, Notched | >= 5.34 J/cm | >= 10.0 ft-lb/in | ASTM D256 |
Buckeye Polymers BP FLEX D6020 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 5.34 - 10.7 J/cm | 10.0 - 20.0 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Izod Impact, Notched | 5.34 - 6.41 J/cm | 10.0 - 12.0 ft-lb/in | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm |
10.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 8150 Rigid PVC, Extrusion & Molding Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |