Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Network Polymers NPP 25-2010

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 25-2010.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ASTM D785
Tensile Strength, Yield 17.9 MPa
2600 psi
2 in per min; ASTM D638
Elongation at Yield 20 %
20 %
chs 2 in/min; ASTM D638
Flexural Modulus 0.772 GPa
112 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Gardner Impact >= 27.1 J

@Temperature -18.0 °C
>= 20.0 ft-lb

@Temperature -0.400 °F
Gardner
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648