Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos K38-20-188 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos K38-20-188 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
K38-20-188 is a natural, UV stabilized, medium density polyethylene resin designed specifically for use with an approved Ineos North America yellow masterbatch to produce pipe or tubing for natural gas distribution. The resulting formulation, known as K38-20X2091, is recognized by the Plastics Pipe Institute as having a PE 2708 (formerly PE 2406) and PE 80 rating. It exhibits excellent long term stress life and outstanding environmental stress crack resistance.Cell Classification 234360D.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Natural; ASTM D4883
Environmental Stress Crack Resistance >= 5000 hour
>= 5000 hour
Condition B; 10%; ASTM D1693
>= 5000 hour
>= 5000 hour
Condition C; ASTM D1693
>= 5000 hour
>= 5000 hour
Pipe Ring; ASTM F1248
Melt Flow 0.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
PENT >= 500 hour
>= 500 hour
Notch Tensile; ASTM F1473
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
2 in/min; ASTM D638
Tensile Strength, Yield 19.3 MPa
2800 psi
2 in/min; ASTM D638
Elongation at Break >= 800 %
>= 800 %
2 in/min; ASTM D638
Flexural Modulus 0.689 GPa
100 ksi
2% Secant - Method 1; ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Descriptive Properties Value Comments