Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.81 J/cm | 9.01 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Izod Impact, Notched | 4.81 J/cm @Temperature -50.0 °C |
9.00 ft-lb/in @Temperature -58.0 °F |
0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Izod Impact, Notched | 4.81 J/cm @Temperature -50.0 °C |
9.00 ft-lb/in @Temperature -58.0 °F |
0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | Crosswise; ASTM D256 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
Ineos TUB 121 HDPE TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind.. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R922 PC/ABS Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS 8800 Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
9.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 9301 Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
9.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS/PC 7901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
9.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers ASAPC 122954H Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers ASAPC TA-45 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P114WO PBT Polyester A high impact polyester with low shrinkage, flame retardant.Data provided by the manufacturer |
|||
Izod Impact, Notched | 4.81 - 5.34 J/cm | 9.00 - 10.0 ft-lb/in | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
Asia Technology Pioneers CAP 501 PP Nanocomposite Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Izod Impact, Notched | 4.81 - 5.87 J/cm | 9.00 - 11.0 ft-lb/in | |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.00 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PCA100 Polycarbonate/ABS Alloy Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
9.00 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |