Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion LR620 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Omni Plastics OmniTuff™ CPP GRC30 Copolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 22.8 °C |
3.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 22.8 °C |
3.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 22.8 °C |
3.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® NL-23CF/000 Nylon 6/12, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Global ABS-305 General Purpose ABS Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | |
MTI ThermoStran® PPA-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU) Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Shuman 210 Polyphenylene Ether Copolymer Alloy Black, Custom Colors. Good impact strength, easy processability, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plaslube® J-50/30/TF/10 Polycarbonate, 30% GFR, 10% PTFE Plaslube glass fiber reinforced polytetrafluorethylene (PTFE) lubricated polycarbonate grades have an excellent balance of mechanical strength characteristics, dimensional stability and wear and fri.. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 892E Extrusion and Blow Molding Grade Homopolymer Polypropylene DescriptionPolyfort® FPP 892E is an extrusion and blow molding grade 20% mineral-filled homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN100L (COND, 50% RH) Nylon 66, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN130GMD2 (COND, 50% RH) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1603 Glass Reinforced Copolymer DescriptionPolyfort® FPP 1603 is a 10% glass reinforced copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Ecomass® 4703ZG92 Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ISO 180/A |
CTC X-PRO TF 2104 GP Recycled Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 2104 GP is a 20% talc reinforced polypropylene homopolymer made of 98% recycled content. It has applications in: automotive, industrial, construction, consumer and lawn & garden products.D.. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPC-GF25 Natural Impact Polypropylene, 25% Glass Reinforced Information provided by Entec |
|||
Izod Impact, Notched | 1.60 - 2.67 J/cm | 3.00 - 5.00 ft-lb/in | |
Bulk Molding Compounds BMC 6241 Glass Reinforced BMC BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availab.. |
|||
Izod Impact, Notched | 1.60 - 4.27 J/cm | 3.00 - 8.00 ft-lb/in | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
injection molded sample; ASTM D256 |
American Polymers API 645-21 Polystyrene API 645-21 is a super high impact polystyrene used in applications requiring a superior level of toughness along with good tensile and flexural properties. On balance this extrusion grade polymer a.. |
|||
Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | |
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.60 J/cm @Diameter 3.17 mm |
3.00 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Acctuf® 3638 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Compounding, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |