American Polymers API 645-21 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer American Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Polymers API 645-21 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
API 645-21 is a super high impact polystyrene used in applications requiring a superior level of toughness along with good tensile and flexural properties. On balance this extrusion grade polymer approaches some ABS properties.Applications: Widely used in sheet stock, housings, profiles and tubing where a high degree of impact over convention PS is needed.Information provided by American Polymers, Inc.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min
3.0 g/10 min
Condition G; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 45
45
ASTM D785
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Tensile Modulus 1.86 GPa
270 ksi
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
injection molded sample; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
172 °F
Annealed; ASTM D648
Vicat Softening Point 95.6 °C
204 °F
ASTM D1525