Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 6.35 mm |
0.600 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 6.35 mm |
0.600 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 924 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Ensinger ENSITEP® PET Polyethylene Terephthalate - Extruded Products
(discontinued **) ENSITEP is an unreinforced, semi-crystalline thermoplastic polyester derived from polyethylene terephthalate. Its excellent wear resistance, low coefficient of friction, high flexural modulus, and .. |
|||
Izod Impact, Notched | 0.320 J/cm @Diameter 0.125 mm, Temperature -20.0 °C |
0.600 ft-lb/in @Diameter 0.00492 in, Temperature -4.00 °F |
bar; ASTM D256 |
Ineos L12Z-00 Polypropylene Impact Copolymer Grade L12Z-00 is a medium melt flow rate, high stiffness and high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA 6/12 (Asia Pacific) LNP* LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2312 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 FR HS BK (Dry) Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.599 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 04003 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific) LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America RX® 3-1-501N-P Mineral Filled Diallyl Phthalate Mineral filled, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Washington Penn Homopolymer Polypropylene 10% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Washington Penn Homopolymer Polypropylene 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.599 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PP-HP12 Homopolymer, 12 Melt Flow This product in intended for general purpose injection molding applications such as caps and closures, resin furniture and consumer products.Information provided by Entec |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W20L1 Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Plastics Group Polifil® RP-PP Polypropylene, Molding Grade Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de.. |