Mechanical Properties Metric English Comments
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 4012 TH Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Nylene® 8100 Unfilled Nylon 6/12
Description: Nylene® 8100 is an unfilled specialty fiber. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation...
Izod Impact, Notched 0.320 J/cm

@Temperature 23.0 °C
0.600 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products T20P250-731UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AS20698 Black
Applications: Automotive trimIP componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.320 J/cm

@Temperature -30.0 °C
0.599 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet)
KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re..
Izod Impact, Notched 0.320 - 4.50 J/cm
0.599 - 8.43 ft-lb/in
Average value: 0.658 J/cm Grade Count:44
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 0.320 - 0.801 J/cm
0.600 - 1.50 ft-lb/in
Average value: 0.564 J/cm Grade Count:15
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Izod Impact, Notched 0.320 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.599 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Therma-Tech™ LC-5000C TC LCP  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Flint Hills P4C6S-193A Homopolymer Polypropylene
Features: Clarified, high Slip and Controlled Rheology. Product does not contain animal derived components. Phthalate-free.Applications: Specialty Injection Molding. Excellent Mold ReleaseInfor..
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
JPJ Technologies PP H35S Homopolymer for Injection Molding
PP H35S is specifically developed for producing injection molding articles for general purpose applications. It gives consistent processability and high gloss in the products. Application: General u..
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be ..
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® POM Acetal
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc.
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PP GB50 50% Glass Beads Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 50% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Plastiblend® PA6 SF80 L
Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (80%)Features: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Washington Penn Homopolymer Polypropylene 10% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Washington Penn Homopolymer Polypropylene 30% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman.
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene
DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman.
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman.
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.599 ft-lb/in

@Thickness 0.125 in
ASTM D256
Entec Hypro™ PP-HP35NS Homopolymer, 35 Melt Flow, Nucleated, Anti-stat
This product is intended for thin-wall injection molding applications such as caps and closures, food containers and consumer products that require high stiffness.Information provided by Entec
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 628 Nylon 6/6, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Notched 0.320 J/cm

@Thickness 6.35 mm
0.600 ft-lb/in

@Thickness 0.250 in
ASTM D256
PlastxWorld DAICEL STYROL® SK50H HIPS
Flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
Conditioned; ASTM D256
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)