Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | dry; ISO 179-1/1eA |
Murtfeldt Murdopol® Nylon 12 Murdopol® has extremely high shock and impact resistance characteristics and good emergency running characteristics thanks to its high wear resistance. The main advantage of this material is its f.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, maximum cold and dry impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend High heat amorphous TPI Blend, Chemical Resistant |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eA |
Pasargad Polymer Peyvand Pasamid 3P-H1000B Nylon 6 Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 eA |
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179 |
SIDPEC EGYPTENE® HD 3840 UA MDPE Rotational Molding Applications:Rotational items: tanks, containers, etc...Injection molded technical parts and closureInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (S.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ 701-15 Polycarbonate Resin Overview: CALIBREâ„¢ 701-15 Series resins are formulated and produced to supply both clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and proce.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 30.0 °C |
9.52 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Charpy Impact, Notched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 MR 209 HWCP Mineral Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® LV-23H PA12-GF23 Product description: Grilamid LV-23H is a 23% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile. Good chemical resistanceGood UV stabili.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® LV-5H PA12-GF50 Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179 |
Chi Mei Polylac® PA-765B ABS - Flame Retardant F.R. Medium Impact |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® RS 6600 Polyamide 6.6 Alloy Polyamide Alloy, Rigid grade, Nylon 6.6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/IeA |
Addiplast Addinyl PMD 20164 Nylon 6 High resistance to repeated impactsInformation provided by Addiplast. |