Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EX9332T PC (Europe-Africa-Middle East) LEXAN* EX9332T polycarbonate resin, MVR (300C/1.2kg) 3 cm3/10min, high viscosity, branched, extrusion, flame retadant, mold release, UV stabilized, transparent, translucent and opaque colors. Materi.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergadur™ PB40 G30 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ1026 PC (Asia Pacific) LEXAN OQ1026 is an optical quality, high purity PC resin optimized for the demanding short cycle times used in DVD production. Advances in technology further enhanced the processability while mainta.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® BFL2000U PC (Asia Pacific) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ASTM D256 |
Iran Petrochemical (PCC) 6040UA High Density Polyethylene HD-6040UA is an ultra-violet light stabilized high density polyethylene injection grade with a narrow molecular weight distribution, specially developed for injection molding of heavy duty parts for.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1/XCF/25 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, Conditioned Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Europe-Africa-Middle East) UV stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ISO 179/1eA |
Styron VELVEXâ„¢ 5250 SC Reinforced Elastomer/PP compound Overview: VELVEXâ„¢ 5250 SC Natural is a reinforced elastomer/PP compound which provides a unique property balance of good stiffness, impact and high heat resistance in combination with a nice so.. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL N110 PPE+HIPS (Europe-Africa-Middle East) NORYL N110 is an unfilled material, with a Vicat B/120 of 115 °C according ISO 306. NORYL N110 has medium temperature resistance and good |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ISO 179-1 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | ISO 179-1 |
Total HDPE SB 1461 High Density Polyethylene - Injection Stretch Blow Molding HDPE SB 1461 is a high density polyethylene with very high stiffness. It has been specifically designed for the manufacture of thin walled containers for foodstuffs (dairy applications particularly.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Akulon® N24-G7 PA6-GF35 35% Glass Reinforced |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 30.0 °C |
5.23 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 30.0 °C |
5.23 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50 Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 30.0 °C |
5.23 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 30.0 °C |
5.23 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30 Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 30.0 °C |
5.23 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 5052 (BGZ-15 FC) PA6-GF15 Product description: Grilon XE 5052 is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber: High impact resistanceGood surface qualityShort cycle timeGood flowabilit.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature -30.0 °C |
5.23 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.10 J/cm² | 5.23 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50 Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 30.0 °C |
5.23 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a.. |
|||
Charpy Impact, Notched | 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Conditioned, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |