Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Triax® 1180 ABS + Polyamide Blend (Conditioned)
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business r.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® BDT5510 ABS Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® H701 Medium heat resistance, high impact strength. ,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | DIN 53453 |
IRPC Polimaxx Polene GA3750 High Density Polyethylene CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND G3240A PP SABIC® PPcompound G3240A is a general purpose, 40% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 139448304. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | ISO Data, Low Temp |
Styron CALIBRE™ 200 10 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | dry; ISO 179 |
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber Description: Medium viscosity, dry impact resistant PA 6, 15% glass fiber reinforced and improved surface gloss.Application: For molding parts with good stiffness and high dimensional stability.In.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | ISO 179 |
Total PPC 5660 Propylene, Heterophasic Copolymer ATOFINA Propylene 5660 is heterophasic copolymer. PPC 5660 is characterized by a medium fluidity offering a combination of ease of processing and good manufactured article properties in application.. |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature 30.0 °C |
6.19 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TR 90 PAMACM12 Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 4174 black 9992 PA1010-GF30 Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010.. |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | ISO 179-2 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TR 90 LS PAMACM12 Product description: Grilamid TR 90 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LS natural contains a processing a.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | cond.; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-30 Polyamide 6 - Natural High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa.. |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature 23.0 °C |
6.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact, Notched | 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Charpy Impact, Notched | 1.30 J/cm² | 6.19 ft-lb/in² | ISO 179/1eA |
Borealis Daplen™ KB4436 TPO Compound Daplen KB4436 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen KB4436 is a material with excellent impact/stiffness ratio. Thanks to its low the.. |