Material Notes:
Product description: Grilamid XE 4174 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4174 black 9992 are: PA1010 Polymer fully based on renewable raw materialsvery low water absorptiongood chemical and UV resistancegood toughnesseasy processing Grilamid XE 4174 black 9992 is particularly suitable for the manufacturing of technical injection molded parts in the application fields of: AutomotiveElectrical & Electronic goodsMechanical engineeringSports & leisure goodsDomestic appliancesInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
Water Absorption 1.6 %
1.6 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 115 MPa
16700 psi
conditioned; ISO 2039-1
150 MPa
21800 psi
dry; ISO 2039-1
Tensile Strength at Break 120 MPa
17400 psi
conditioned; ISO 527-1/-2
140 MPa
20300 psi
dry; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 7.20 GPa
1040 ksi
conditioned; ISO 527-1/-2
7.80 GPa
1130 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
8.00 J/cm²
38.1 ft-lb/in²
dry; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
dry; ISO 179/1eA
1.30 J/cm²
6.19 ft-lb/in²
conditioned; ISO 179/1eA
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 125 °C
257 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 40.0 kV/mm
1020 kV/in
dry; IEC 60243-1
40.0 kV/mm
1020 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Exterior
Fuel systems
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Lighting
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide