Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/1eA |
Radici Raditer® B RVA 300 Polybutylene Terephthalate with 30% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 H-SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/1eA |
Pasargad Polymer Peyvand Pasamid 3P-H2000B1 Nylon 66 Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact, Notched | 1.00 - 1.36 J/cm² | 4.76 - 6.47 ft-lb/in² | Average value: 1.11 J/cm² Grade Count:4 |
Overview of materials for Chlorinated PVC (CPVC) This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latene® AG7H G/30 PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Glass fibers. Good thermal propertiesAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | |
LATI Latilub 66-20T G/20 PA66, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with .. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33 Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Charpy Impact, Notched | 1.00 J/cm² @Temperature 30.0 °C |
4.76 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® LBV-30H FWA nat PA12-GF30 Product Description: Grilamid LBV-30H FWA natural is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | ISO 179/IeA |
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |