Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
Polycasa Acryl® G 87 E Acrylic Grade for extruding semi-finished products such as twin-strapped panels, profile and tubes, as well as injection molding of watch glasses, dishes, bowls, water-tap hand grips and bathroom fittings, .. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Charpy Impact, Notched | 0.200 - 0.300 J/cm² | 0.952 - 1.43 ft-lb/in² | Injection; ISO 179/ 1eA |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Charpy Impact, Notched | 0.200 - 0.400 J/cm² | 0.952 - 1.90 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Charpy Impact, Notched | 0.200 - 0.400 J/cm² | 0.952 - 1.90 ft-lb/in² | Injection and Compression; ISO 179/1eA |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH B8075 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
(d Melamine/phenolic molding compound, inorganically filled, glass fiber reinforced, good temperature stability, high level of mechanical properties, copper adhesive, flammability UL 94/V-0/1.6 mm (not.. |
|||
Charpy Impact, Notched | 0.200 - 2.00 J/cm² | 0.952 - 9.52 ft-lb/in² | Average value: 0.650 J/cm² Grade Count:7 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Charpy Impact, Notched | 0.200 - 0.200 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 0.952 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.200 J/cm² Grade Count:4 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ASTM D256 |
Plenco 7466 Phenolic, Nodular, Injection Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07466 is a flock cotton and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. UL recognized under component file E406.. |
|||
Charpy Impact, Notched | 0.200 - 1.80 J/cm² | 0.952 - 8.57 ft-lb/in² | Average value: 0.953 J/cm² Grade Count:60 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 0.200 - 1.70 J/cm² | 0.952 - 8.09 ft-lb/in² | Average value: 0.635 J/cm² Grade Count:40 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Charpy Impact, Notched | 0.200 J/cm² - NB @Temperature -40.0 - 30.0 °C |
0.952 ft-lb/in² - NB @Temperature -40.0 - 86.0 °F |
Average value: 0.936 J/cm² Grade Count:226 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® Frost 952 70 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
LATI Latamid 12 H FE90 PA 12, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Magnetizable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
LATI Latistat 62-08 PA6 Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Luran® 378 P Crystal Clear Transparent SAN Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 30.0 °C |
0.952 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GTR 45 PA6I/6T Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® L 20 EC PA12-CD25 Product Description: Grilamid L 20 EC is an electrically conductive, medium viscosity injection molding product, based on Polyamid 12 (PA12). Grilamid L 20 EC is heat stabilized, easy to process wit.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO 179 |
Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | ISO Data |
Dow Tyril® 880B SAN TYRIL® 880B SAN copolymer combines the high levels of chemical resistance, heat resistance and overall strength of 880 resin with improved mold flow and mold release characteristics.Data provided b.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 30.0 °C |
0.952 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® G 25 PA6I/6T Product description: Grivory G 25 is a very high viscous amorphous copolyamide. It is suitable for injection stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of .. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
LATI Latilub 95-25GR CE/10 PSU, Mineral Fiber Reinforced, Graphite Filled Self-lubricating product based on Polysulfone (PSU). Graphite. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® FK 005 Polypropylene Homopolymer Applications include injection molding and thermoforming. Antistatic stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability, good mechanical properties.Application areas: Insulating flanges, sealings, pulleys.Information p.. |