Mechanical Properties Metric English Comments
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 105 - 230 MPa
15200 - 33400 psi
Average value: 185 MPa Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Ball Indentation Hardness 105 MPa
15200 psi
DIN 53456
Ineos Nova S-3222 Medium Impact Compact Polystyrene  (discontinued **)
All mechanical properties measured under standard conditions 50% RH and 23°C.Information provided by NOVA Chemicals.INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture betwee..
Ball Indentation Hardness 105 MPa
15200 psi
DIN 53456
Global PP-1111-R Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-electrical/electronic Information provided by Global Polymers Corporation.
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid
PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera..
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Ineos ABS Lustran® ABS E211 LNS013 Pellets (a-methylstyrene-SAN-modified), Extrusion Grade
Lustran® ABS E211 LNS013 is extrusion grade with high heat resistance. It is used for the production of molded plastic articles.
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Styrolution Novodur® E211 ABS
Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Styrolution Novodur® H604 ABS
Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Styrolution Novodur® H605 ABS
Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Styrolution Novodur® H702 ABS
Novodur H702 is a high heat, high gloss injection molding grade with very good flowabilityInformation provided by Styrolution
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Styrolution Novodur® M201AS ABS
Novodur M201AS is a medium impact, high gloss injection molding grade with improved chemical resistanceInformation provided by Styrolution
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Styrolution Novodur® M203FC ABS
Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution
Ball Indentation Hardness 105 MPa
15200 psi
DIN 53459
Styron Pulse® A35-105 PC/ABS
PULSEâ„¢ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f..
Ball Indentation Hardness 105 MPa
15200 psi
DIN 53459
Styron Pulse® A35-110 PC/ABS
PULSEâ„¢ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p..
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
Styrolution Novodur® H801 ABS / PC
Novodur H801 is a high heat injection molding grade with high impact strength and reduced emission.Information provided by Styrolution
Ball Indentation Hardness 105 MPa
15200 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30
Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi..
Ball Indentation Hardness 105 MPa
15200 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4129 black 9020 PA610
Product description: Grilamid XE 4129 black 9020 is a high viscosity Polyamide 610 especially suitable for extrusion applications. A characteristic of tubes made out of this material is the high res..
Ball Indentation Hardness 105 MPa

@Load 36.5 kg,
Time 30.0 sec
15200 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® N2640 E2 POM
Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber
CENTROPLAST BC NF 15 is made of CO2-neutral, sustainable raw-materials with 15% natural fiber.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegr..
Ball Indentation Hardness 105 - 125 MPa
15200 - 18100 psi
ISO 2032-N132
Adamas Adalon® 704 PTFE, Long Carbon Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 105 MPa

@Load 36.5 kg,
Time 30.0 sec
15200 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® N2650 Z2 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Ball Indentation Hardness 105 MPa

@Time 30.0 sec
15200 psi

@Time 0.00833 hour
DIN 53 456
Hippe PVDF
Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol..
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT
Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF
Ball Indentation Hardness 105 MPa
15200 psi
ISO 2039-1
CENTROPLAST BC Organic Thermoplastic
CENTROPLAST BC is made of CO2-neutral, sustainable raw-materials.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegradable by composting accordin..