Mechanical Properties Metric English Comments
Ball Indentation Hardness 75.0 MPa
10900 psi
ISO2039.1 DIN.53456
Omnia Plastica PP Polypropylene
The mechanical features of PP are better than those of PE H.D. It withstands attack by alkali and acids and consequently it is widely used for components in the chemical industry when a moderate str..
Ball Indentation Hardness 75.0 MPa
10900 psi
ISO2039.1 DIN.53456
Omnia Plastica PVC Polyvinylchloride
A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.Fea..
Ball Indentation Hardness 75.0 - 82.0 MPa
10900 - 11900 psi
Average value: 79.3 MPa Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Ball Indentation Hardness 75.0 - 220 MPa
10900 - 31900 psi
Average value: 148 MPa Grade Count:10
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Ball Indentation Hardness 75.0 - 210 MPa
10900 - 30500 psi
Average value: 141 MPa Grade Count:6
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Ball Indentation Hardness 75.0 MPa
10900 psi
Conditioned; ISO 2039-1
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
Ball Indentation Hardness 75.0 MPa

@Load 36.5 kg,
Time 30.0 sec
10900 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Terlux® 2812 HD MABS
Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15
Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b..
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® EBV-2H PA6-GF20
Product description: Grilon EBV-2H is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 20% glass fibers. Grilon EBV-2H has the following important properties: High melt streng..
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSGZ-15 PA666-GF15
Product description: Grilon TSGZ-15 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 15% glass fibers. Grilon TSGZ-15 has the following important p..
Ball Indentation Hardness 75.0 MPa
10900 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-709S ABS - Extrusion
Super Impact Extrusion
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® LKN-3H PA12-GB30
Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g..
Ball Indentation Hardness 75.0 MPa
10900 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-764 ABS - Flame Retardant
F.R. Weather Resistant
Ball Indentation Hardness 75.0 - 290 MPa
10900 - 42100 psi
Average value: 160 MPa Grade Count:19
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TS V0 X PA666 FR
Product description: Grilon XE 5030 is a heat stabilized, flame retardant and self-extinguishing injection molding grade on the basis of PA6-PA66-alloy. Grilon XE 5030 features the following main pr..
Ball Indentation Hardness 75.0 MPa
10900 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BM-30/2 PA6-MD30
Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App..