Ball Indentation Hardness 50.0 MPa
7250 psi
ISO2039.1 DIN.53456
Omnia Plastica PE 500 - Polyethylene 500
Polyethylene with a molecular weight of ± 500,000. PE 500 is more rigid than the high molecular weight polyethylene and it is therefore more suitable for mechanical applications. The friction coeff..
Ball Indentation Hardness 50.0 - 160 MPa
7250 - 23200 psi
Average value: 138 MPa Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Ball Indentation Hardness 50.0 MPa
7250 psi
ISO 2039-1
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade
PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS.
Ball Indentation Hardness 50.0 MPa
7250 psi
Conditioned; ISO 2039-1
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding
Ball Indentation Hardness 50.0 MPa
7250 psi
Hc 30; ISO 2039; partially
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned
Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH
Ball Indentation Hardness 50.0 MPa
7250 psi
358 N/30s; ISO 2039
Borealis Daplen™ EE188AI Polypropylene TPO Compound
Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
Ball Indentation Hardness 50.0 MPa
7250 psi
358 N/30s; ISO 2039
Borealis Daplen™ EE189AI Polypropylene TPO Compound
Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
Ball Indentation Hardness 50.0 MPa
7250 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610
Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati..
Ball Indentation Hardness 50.0 MPa
7250 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 2S 25 W 20 HL X nat PA610
Product Description: Grilamid 2S 25 W 20 HL X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified and plasticized Polyamide 610, espcailly suitable for extrusion applic..
Ball Indentation Hardness 50.0 MPa
7250 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 2S 25 W 20 X black 9992 PA610-I
Product Description: GRILAMID 2S 25 W 20 X black 9992 is a semi-flexible high viscosity heat and impact modified polyamide 610, especially suitable for extrusion applications. This PA610 product is ..
Ball Indentation Hardness 50.0 MPa
7250 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 2S 25 W 20 X nat PA610-I
Product Description: GRILAMID 2S 25 W 20 X natural is a semi-flexible high viscosity heat and UV stabilized, impact modified polyamide 610, especially suitable for extrusion applications. This PA610..
Ball Indentation Hardness 50.0 MPa
7250 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4129 black 9020 PA610
Product description: Grilamid XE 4129 black 9020 is a high viscosity Polyamide 610 especially suitable for extrusion applications. A characteristic of tubes made out of this material is the high res..
Ball Indentation Hardness 50.0 MPa
7250 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-K25 PTFE
Based on Tarflen SM1 reinforced with 25% coke for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032-N132
Adamas Adalon® 237 PTFE, 25% Glass Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032-N132
Adamas Adalon® 252 PTFE, 28% Glass Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032-N132
Adamas Adalon® 406 PTFE, 15% PEEK
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032
Adamas Adalon® 509 PTFE, 3% MoS2
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 MPa
7250 psi
value at 30 sec.; ISO 2039-1
CENTROPLAST CENTROLEN PE-HD Polyethylene high density
This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor..
Ball Indentation Hardness 50.0 MPa
7250 psi
ISO 2039
Orbilan ORBILAN® PE 500 HMW-PE
Orbilan PE 500 plastic is used as cutting boards for the food industry and gastronomy, in refrigeration chambers as ram protection and for swing doors as well as at sports grounds for sheets or hand..
Ball Indentation Hardness 50.0 - 160 MPa
7250 - 23200 psi
Average value: 132 MPa Grade Count:5
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Ball Indentation Hardness 50.0 - 190 MPa
7250 - 27600 psi
Average value: 119 MPa Grade Count:32
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Ball Indentation Hardness 50.0 - 60.0 MPa
7250 - 8700 psi
ISO 2032-N132
Adamas Adalon® 266 PTFE, Mineral/Glass Bubbles Filler
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 - 52.0 MPa
7250 - 7540 psi
ISO 2032
Adamas Adalon® 600 PTFE, Boro Nitruro
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 MPa
7250 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BZ 1 PA6
Information provided by EMS Grivory
Ball Indentation Hardness 50.0 MPa
7250 psi
H385/30; ISO 2039
Borealis Daplen™ KSX65T20 Polypropylene Compound 20% Mineral Filled
Daplen KSX65T20 is a 20% mineral filled grade intended for injection molding. Daplen KSX65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSX65T20 offe..