Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTROLEN PE-HD Polyethylene high density

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROLEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROLEN PE-HD Polyethylene high density.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Water Absorption at Saturation 0.010 %
0.010 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 50.0 MPa
7250 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 30.0 MPa
4350 psi
v = 50 mm/min; ISO 527-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-2
Tensile Modulus 1.00 GPa
145 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.370 W/m-K
2.57 BTU-in/hr-ft²-°F
Melting Point 130 - 135 °C
266 - 275 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 80.0 °C
176 °F
Long Term
120 °C
248 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-2
Vicat Softening Point 80.0 °C
176 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -75.0 °C
-103 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 6.00 mm
HB

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 2.3

@Frequency 100 Hz
2.3

@Frequency 100 Hz
IEC 60250
2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 45.0 kV/mm
1140 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.00020

@Frequency 100 Hz
0.00020

@Frequency 100 Hz
IEC 60250
0.00020

@Frequency 1e+6 Hz
0.00020

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Food Compliance yes
BGVV
yes
FD A