Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 13500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
SABIC Innovative Plastics Cycoloy® CH6310 PC+ABS (Asia Pacific)
CH6310 is a high heat, high flow PC/ABS resin, with nonbrominated, nonchlorinated flame retardant system. All color available.
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
SABIC Innovative Plastics Cycoloy® MC5300 PC+ABS (Asia Pacific)
Cycoloy MC5300 resin is a high heat, flame retardant PC/ABS blend. MC5300 resin passes UL-94 listing of 1.5mm V0 and 2.5mm 5VB. The balance of good flow, impact performance and heat resistance makes..
Flexural Strength 93.0 MPa
13500 psi
Quadrant EPP Acetron® MD POM-C + metal detectable additive, extruded (ISO Data)
Metal detectable POM-C grade High mechanical strength, stiffness and hardness Excellent resilience Good creep resistance High impact strength, even at low temperatures Very good dimensional stabilit..
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized
Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical..
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate
Information provided by Ravago
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
PolyOne Geon™ Vinyl Fittings 210(HS) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact
Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica..
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
PolyOne Lubri-Tech™ AS-20GF/05T Acrylonitrile Butadiene Styrene (ABS), Glass Filled, PTFE Lubricated  (discont
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
PolyOne Lubri-Tech™ BB-10GF/5T PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Kostat ICP-STAT ICS-1000 PC Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC (Asia Pacific)
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Flexural Strength 93.1 MPa
13500 psi
SGL Carbon Group EK 3105 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Flexural Strength 93.0 MPa
13500 psi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific)
A new high flow GTX designed for under-the-hood applications such as power distribution boxes, relay boxes and junction boxes. Developmental name: EXNX0151.
Flexural Strength 93.0 MPa
13500 psi
ISO 178
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT
LNP* STAT-LOY* WF306C is a compound based on PBT resin containing 30% Glass Fiber. Added features of this material include: Antistat, Clean Compound System.
Flexural Strength 93.0 MPa
13500 psi
2mm/min; ISO 178
Teijin Panlite® LV-2250Z Transparent and Weather Resistant grade Polycarbonate Resin
Typical injection molding grade that has weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of electric, electronic, business machine and industrial equipment com..
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
A. Schulman POLYFORT™ FPP 3710 Glass Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 3710 is a 45% glass filled homopolymer polypropylene product. Information provided by A. Schulman.
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Plenco 2308 Phenolic, Granular, Compression Molded
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai..
Flexural Strength 93.1 MPa
13500 psi
TriStar Ultracomp UC-200 Composite Bearing
Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m..
Flexural Strength 93.1 MPa
13500 psi
ASTM D638
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene
Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature..
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Ecomass® 1850ZD88 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers
Flexural Strength 93.0 MPa
13500 psi
2 mm/min; ISO 178
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded
Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Entec Hylex® P1307L1 HB Polycarbonate
UV Stabilized, Low Flow, Mold Release, Water ClearInformation provided by Entec.
Copyright © lookpolymers.com All Rights Reserved