Ravago Manufacturing Americas Hylex® P1310L Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylex®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ravago Manufacturing Americas Hylex® P1310L Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Entec.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
24-Hr Immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
10 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength 69.6 MPa
10100 psi
ASTM D638
Elongation at Break 115 %
115 %
ASTM D638
Flexural Strength 93.1 MPa
13500 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
<br>@Thickness 3.17 mm
15.0 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ASTM D648
Vicat Softening Point 154 °C
310 °F
ASTM D1525
Flammability, UL94 V-2
<br>@Thickness 1.50 mm
V-2
<br>@Thickness 0.0591 in
V-2
<br>@Thickness 3.00 mm
V-2
<br>@Thickness 0.118 in
V-0
<br>@Thickness 6.00 mm
V-0
<br>@Thickness 0.236 in
Optical Properties Metric English Comments
Refractive Index 1.585
1.585
ASTM D542
Haze 0.50 - 0.80 %
<br>@Thickness 3.17 mm
0.50 - 0.80 %
<br>@Thickness 0.125 in
ASTM D1003
Transmission, Visible 89 - 91 %
<br>@Thickness 3.17 mm
89 - 91 %
<br>@Thickness 0.125 in
Electrical Properties Metric English Comments
Electrical Resistivity 4.00e+16 ohm-cm
4.00e+16 ohm-cm
ASTM D257
Dielectric Strength 16.1 kV/mm
<br>@Thickness 3.17 mm
410 kV/in
<br>@Thickness 0.125 in
in Air; ASTM D149
Arc Resistance 120 sec
120 sec
ASTM D495