3D Systems Accura® 40 Plastic for SLA® Systems

Category Polymer , Rapid Prototyping Polymer
Manufacturer 3D Systems Corporation
Trade Name Accura®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3D Systems Accura® 40 Plastic for SLA® Systems.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
40 Accura "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsHigh temperature testing:Automotive "under-the-hood" partsIntake manifoldsLighting components and accessoriesHVAC componentsParts where additional assembly or machining operations may be required (self-tapping screws, drilling, etc.)Thin-wall enclosuresMaster patterns for RTV/silicone moldingWind-tunnel modelsSnap-fit assembliesFeaturesStiffness matches nylon 6:6High heat resistance without brittlenessGood durabilityOutstanding accuracy with minimal distortionFully developed and tested build stylesAll information provided by 3D Systems.
Physical Properties Metric English Comments
Density 1.16 g/cc

@Temperature 25.0 °C
0.0419 lb/in³

@Temperature 77.0 °F
Liquid
1.19 g/cc

@Temperature 25.0 °C
0.0430 lb/in³

@Temperature 77.0 °F
Solid
Viscosity 485 cP

@Temperature 30.0 °C
485 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength, Yield 57.0 - 61.0 MPa
8270 - 8850 psi
ASTM D638
Elongation at Break 4.8 - 5.1 %
4.8 - 5.1 %
ASTM D638
Tensile Modulus 2.628 - 3.321 GPa
381.2 - 481.7 ksi
ASTM D638
Flexural Strength 92.8 - 97.0 MPa
13500 - 14100 psi
ASTM D790
Flexural Modulus 2.618 - 3.044 GPa
379.7 - 441.5 ksi
Izod Impact, Notched 0.223 - 0.299 J/cm
0.418 - 0.560 ft-lb/in
ASTM D256
Penetration 6.6
6.6
mils; Viper/SLA 3500
6.6
6.6
mils; SLA 5000
6.8
6.8
mils; SLA 7000
Thermal Properties Metric English Comments
CTE, linear 87.0 µm/m-°C

@Temperature 0.000 - 20.0 °C
48.3 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
187 µm/m-°C

@Temperature 90.0 - 150 °C
104 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 51.0 - 54.0 °C
124 - 129 °F
ASTM D648
101 - 114 °C
214 - 237 °F
with 160ºC thermal postcure; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.0 - 49.0 °C
109 - 120 °F
ASTM D648
Glass Transition Temp, Tg 62.0 - 65.6 °C
144 - 150 °F
DMA, E"
Descriptive Properties Value Comments
Appearance Clear amber
Critical Exposure (mJ/cm²) 20.1
SLA 7000
20.2
SLA 5000
21.7
Viper/SLA 3500
Tested Build Styles EXACT™, Exact HR, FAST™, ThinLayer™
Users viewing this material also viewed the following: