Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.0 MPa | 5080 psi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Plastcom SLOVALEN PC 12 T 30 TS PP reinforced with 30% mineral filler Features: Modified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in t.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Plastcom SLOVALEN PC 13 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in the.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Plastcom SLOVALEN PH 96 FRD 1 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM D790 |
SABIC PS 325 High Impact Polystyrene for Injection Molding Product Description: High Impact Polystyrene PS 325 is manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resis.. |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PP CIQ10015ER UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPC K20010 PP, 10% Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPC K5025 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Pyrotek NT-C Electrical Insulating Material NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro.. |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB SCANFILL Injection CPC15051 PP/PE, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 35.0 - 60.0 MPa | 5080 - 8700 psi | Transverse |
Quadrant Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev.. |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPH B8065 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Nilit FRIANYL C73 S10 Nylon 6.6/6 for injection molding Nylon 6.6/6 for injection molding, medium viscosity, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Fiberfil® M-2450 BK9083 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MX01767C PP LNP* STAT-KON* MX01767C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MX10301C PP LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Polyram RamOfin PPC101 Polypropylene Copolymer, Heat Stabilized Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Polyplastics Duracon® TD-30 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Tech.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L Calcium Reinforced |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C40L Calcium Reinforced |
|||
Flexural Strength | 35.0 MPa | 5080 psi | cond.; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM Test |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPC T1020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Polyram RamOfin PPC104 Polypropylene Copolymer Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |