Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler
Manufacturer Polykemi AB
Trade Name POLYfill
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Polykemi AB POLYfill PPC K5025 Polypropylene Copolymer, Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Filler Content 25 %
25 %
±2%; Polykemi
Melt Index of Compound 5.0 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
5.0 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 20.0 MPa
<= 2900 psi
ISO/R527
Elongation at Yield 7.0 %
7.0 %
ISO/R527
Flexural Strength <= 35.0 MPa
<= 5080 psi
ISO 178
Flexural Modulus 1.60 GPa
<br>@Temperature 23.0 °C
232 ksi
<br>@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.500 J/cm²
<br>@Temperature 23.0 °C
2.38 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
120°C/h; ISO 75/1
Vicat Softening Point 70.0 °C
<br>@Load 5.001 kg
158 °F
<br>@Load 11.03 lb
50°C/h; ISO 306
135 °C
<br>@Load 1.00 kg
275 °F
<br>@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 HB
<br>@Thickness 1.60 mm
HB
<br>@Thickness 0.0630 in
Glow Wire Test 750 °C
<br>@Thickness 2.00 mm
1380 °F
<br>@Thickness 0.0787 in
IEC 695-2-1
Processing Properties Metric English Comments
Melt Temperature 205 - 260 °C
401 - 500 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
2 - 4 hour
2 - 4 hour
in desiccant air dryer
Injection Pressure 40.0 - 110 MPa
5800 - 16000 psi
Back Pressure 1.00 - 2.00 MPa
145 - 290 psi
Descriptive Properties Value Comments
Holding Pressure () 20-40
% of injection pressure
Injection Speed () High