Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Oxford Polymers Oxtron PPS-XT-40GF PPS, 40% Glass Reinforced Product Description: Glass Fiber (40% Reinforced), Polyphenylene sulfide injection molding grade based alloy. Processing and Delivery Form: Pellets and Injection MoldingAppearance: Natural off-whit.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
PolyOne Edgetek® PK-20GF/000 Polyetheretherketone (PEEK), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
PolyOne Edgetek® SF-20CF/000 Polyphenylene Sulfide (PPS)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M40 ML2 GY 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and He.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF30 HR L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Lubricated and Hydroly.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: LubricatedTPCI# 8682101Information provided by TP Composite.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated TPCI# 8263101Information provided by TP Composit.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 LE BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesAppearance: BlackTPCI#7762101Information provided by TP Compos.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF33 TS15 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant and PTFE Lubricant(15%)Features: Lubricated, Good Wear R.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 HS L GY 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Techmer ES Plastiblend® PA6 GF20 RM L BK Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedBlackTPCI# 9718102Inf.. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Chase Plastics CP Pryme® N340HSL (DAM) Nylon 6 (Utility Grade), 40% Glass Fiber Reinforced, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Flexural Strength | 221 MPa | 32000 psi | IPC TM-650 2.4.4 |
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal .. |
|||
Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 221 MPa | 32000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |