| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.52 g/cc | 1.52 g/cc | ASTM D792 |
| Water Absorption | 0.030 % | 0.030 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 172 MPa | 25000 psi | ASTM D638 |
| Elongation at Break | 2.0 % | 2.0 % | ASTM D638 |
| Flexural Strength | 221 MPa | 32000 psi | ASTM D790 |
| Flexural Modulus | 21.7 GPa | 3150 ksi | ASTM D790 |
| Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 10 - 100 ohm-cm | 10 - 100 ohm-cm | ASTM D648 |
| Surface Resistivity per Square | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D648 |