Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 53.0 MPa | <= 7690 psi | ISO 178 |
Polykemi AB POLYfill PPH TS15040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir RC 600 Polystyrene Special medium impact polystyrene grade exhibiting very high gloss. This grade is designed to be used in injection moulding where an excellent surface finish is requiredApplications: Examples of ap.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2 mm/min; ISO 178 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ASTM D790 |
LG Chemical HI855HS PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTU PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency, UV cut, and superior cleanliness for advanced semiconductor packaging applications |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF) LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VC-0830 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP V1000UXC PA LNP* Thermotuf* V1000UXC is a compound based on Nylon resin. Added features of this material include: UV Stabilized. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON 9X08403C Liquid Crystal Polymer (LCP) LNP* STAT-KON* 9X08403C is a compound based on Liquid Crystal Polymer (LCP) resin containing Carbon Fiber. Added features of this material are: Clean Compounding System, High Temperature, Flame Re.. |
|||
Flexural Strength | 53.0 MPa @Thickness 3.20 mm |
7690 psi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 515 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any colorProcessing Injection molding Extrusion Applications Electrical switch boards MCB distribution bo.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
Polyplastics Duracon® TD-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
Eurostar Star L POM D61 POM, Injection Molded Star L POM D61 is a PTFE/Silicone Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334G5M25CL Glass/Mineral Reinforced Coupled |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336G10CL Glass Reinforced Coupled |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ASTM D790 |
Aclo Accucomp ABS ABS804L High Impact Grade |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436G15M15CL Glass/Mineral Reinforced Coupled |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermotuf V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 53.0 MPa | 7690 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific) LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |