Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 181 MPa | 26300 psi | ASTM D790 |
PolyOne Edgetek® X AS-40CF/000 Natural SE Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Strength | 181 MPa | 26300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI (Asia Pacific) LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 181 MPa | 26300 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive. |
|||
Flexural Strength | 181 MPa | 26300 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON WE002 PBT LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 181 MPa | 26300 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON WE002 PBT (Asia Pacific) LNP STAT-KON* WE002 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 181 MPa | 26300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific) DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Flexural Strength | 181 MPa | 26300 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 181 MPa | 26300 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific) LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 181 MPa | 26300 psi | ASTM D790 |
Unitika AXG-1500-300 Conditioned Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Flexural Strength | 181 MPa | 26300 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Flexural Strength | 181 MPa | 26300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable. |